Getting finning on photopolymers?




One good fix for this is use a 1,600 degree burnout rather than the suggested 1250. Docs will fuse into a far stronger material and withstand the expansion pressure presented by resin models. Thanks to Manuel Novo for this tip which came from a new ultra smooth product from Envision. The new material is a kind of orange color and is very highly detailed. The picture is just a good casting done in Docs and 95oPd.

Comments

Popular posts from this blog

Resin Cad Cam or Photopolymers

For those most difficult resin Cad-Cam models... If you are using this material to simply overcome the defects that you encounter from the use of carving or RP waxes, you can just as well use a normal jewelry burnout cycle in the same oven as your normal daily production flasks. Method B: (Smaller flasks or small flask-less castings) Note: Casting flask-less is ideal with this type of material · Program your oven controller for a ramp rate from 4 degrees per minute to a maximum of 10 degrees per minute. This investment material is very resistant to shock so your ramp up speed can be faster than with gypsum-bonded investment. · About 1 hour after investing, put the flask into an oven that is preheated to about 300 o F (150 o C), with the wax button facing down. · Ramp directly up to your top burnout temperature of about 1350 o F - 1600 o F, depending on the metal you are burning out. For photopolymer...

If You Need To Order Docs...

If you need to order Docs you can call 213-675-6178, or email orders@talladium.com  Please supply address, number of boxes you need and a credit card or COD arrangements for your account. Any questions at all, call Daniel. 213-675-6178
Change is here. Please visit  https://docscastingplaster.com/  for future updates and news on Docs.